Under the long-term influence of various external factors of enamel reactor, it is inevitable that there will be some losses, such as rust and surface wear. When these conditions occur in the reactor, the repair should be carried out in time, otherwise, letting it develop will only cause more serious losses. In the face of these situations, repair can be carried out by means of rust removal, painting, etc., to stop the damage in time and make it a new look. However, in order to make the repair effect reach the standard, the following matters should be paid more attention when removing rust and painting enamel reactor.
1. Paint, grease, oxide, etc. shall be removed by sand blasting. The enamel reactor surface shall be approved and recorded by relevant personnel before anti-corrosion and painting.
2. Before painting, the primer shall be fully mixed, and the dust and moisture on the surface shall be removed with cotton yarn or compressed air. The enamel reactor that is derusted on the same day shall be painted with a primer on the same day. Before the primer is dry, the primer shall not be brushed twice, and the primer on the pipe surface shall be uniform without leakage.
3. Before sand blasting and derusting, check the ovality, wall thickness and material of all equipment to see if they meet the material specifications, otherwise they shall not be used.
4. Rust removal and painting of enamel reactor shall be carried out according to drawings and specifications.
Therefore, when cleaning the paint enamel reactor, we must pay more attention to the contents mentioned above. After the damaged parts of the reactor are repaired, we suggest that you can do some more protection and maintenance work, which can not only consolidate the repair effect of cleaning and painting, but also reduce the incidence of faults in the reactor and improve its use effect.